The results of the manifold block were beyond expectation due to reduced build time, less material consumption reduced support removal and post-processing increased efficiency and no leakage in operation.
Improved Performance: Structural integrity was drastically enhanced, and the deflections were 75%.
Weight Reduction: Reduction of component weight from 3.61 kg to 0.54 kg leading to 75% mass reduction.
Time Frame: The complete redesign to realize the lifecycle for the manifold block was reduced to 8 hours against conventional method of 30 hours.
Improved flow efficiency up to 55%: The horizontal holes are no longer needed, the fluid can now flow around the corner and is not disturbed by corners and edges.